Characterization and testing of glass-ceramic sealants for protonic ceramic electrolysis cells applications

S. Anelli,A. Baggio,D. Ferrero,D. Schmider,J. Dailly,M. Santarelli,F. Smeacetto
DOI: https://doi.org/10.1016/j.ceramint.2024.02.240
IF: 5.532
2024-02-01
Ceramics International
Abstract:Protonic ceramic electrolysis cells (PCECs) are high-temperature electrolysers (HTEs) which use ceramic electrolytes characterized by high protonic conductivity. Compared with other HTEs (e.g., solid oxide electrolysis cells, SOECs), PCEC devices work at considerably lower temperatures (i.e., 350-600 °C compared with 700-900 °C of SOEC). Nowadays, studies related to PCEC have been confined to the lab scale, with only a few attempts to scale up this technology. A single repeating unit (SRU) or a stack of large area PCEC cells is still a technological challenge and the formulation of appropriate sealants to join ceramic cells and metallic interconnects is necessary to fulfil this task. In this study, three compositions of Si-based glass-ceramic (two Na-rich and one Ba-rich) have been chemically and thermomechanically tested with materials for PCEC electrolyte (Ba(Ce,Zr)1-yMyO3-δ) and a ferritic stainless steel interconnect (FSS, AISI441). Afterwards, the joined sample were characterized using SEM-EDX and XRD. One of the studied compositions, a Si-based glass-ceramic containing also Na and Zr, showed promising results. The results of the microstructural analyses highlighted excellent compatibility with both the BCZY72 electrolyte and the AISI441 stainless steel after joining and ageing of 1000 h at 600 °C in static air. Moreover, this glass-ceramic system has been joined with AISI441 steel and characterized at 600 °C with the application of a voltage and different atmospheres. Good compatibility of the glass-ceramic with the AISI441 was highlighted by the microstructural characterization also in these conditions.
materials science, ceramics
What problem does this paper attempt to address?