Influence of Electrochemically Charged Hydrogen on Mechanical Properties of Ti–6Al–4V Alloy Additively Manufactured by Laser Powder-Bed Fusion (L-PBF) Process

Wangping Wu,Guang He,Jiaqi Huang,Ao Zhang,Xiliang Liu,Zhong Ouyang,Zilong Sun,Li Guan,Song Chu,Peng Li,Peng Jiang,Yi Zhang
DOI: https://doi.org/10.1016/j.msea.2022.144339
2023-01-01
Abstract:Ti-6Al-4V alloy parts were obtained by laser powder bed fusion (L-PBF) process. The influence of electro-chemically charged hydrogen on the microstructure, phase identification, and mechanical properties of as -charged Ti-6Al-4V alloy parts from printing and deposition directions was studied. The impact of hydrogen desorption on L-PBF Ti-6Al-4V alloy parts was characterized with oxygen nitrogen hydrogen analyzer, X-ray diffraction (XRD) and scanning electron microscopy (SEM). The results showed that as-built Ti-6Al-4V alloy was composed of a unique structure of a kind of equiaxed alpha (hcp) + intergranular beta (bcc) dual-phase. The average surface roughness values for Ra and Rq were 10.1 +/- 1.0 mu m and 12.6 +/- 1.3 mu m, respectively. After electro-chemically charged hydrogen, the phase in the part was composed of a solid solution of hydrogen in alpha-phase, and 8-TiH2 and 8-TiHx hydride phases. The mechanical properties of as-printed Ti-6Al-4V alloy part from deposition direction were higher than those of as-built part from printing direction. After electrochemically charged hydrogen, the hydrogen content in the as-built Ti-6Al-4V alloy part increased significantly. The mechanical properties of the as-charged parts from printing and deposition directions were decreased significantly. The susceptibility to hydrogen embrittlement significantly depended on the orientation of additively manufactured Ti-6Al-4V alloy parts, the as-printed part from deposition direction had a higher resistance to hydrogen embrittlement compared with printing direction. After electrochemically charged hydrogen, Ti-6Al-4V alloy parts from printing direction was prone to brittle fracture and form the microcracks in alpha phase or along alpha/beta interface in the as-built part.
What problem does this paper attempt to address?