Vacuum Brazing of AlON and Ti2AlNb with LiAlSiO4 Enhanced Ag–Cu–Ti Composite Fillers: Microstructure, Mechanical Properties and Measurement of Residual Stress

Hao Jiang,Chun Li,Xiaojian Mao,Lei Chen,Wendi Zhao,Xiaoqing Si,Junlei Qi,Zhibo Dong,Jian Cao
DOI: https://doi.org/10.1016/j.msea.2022.143277
2022-01-01
Abstract:In this paper, the AlON ceramic is successfully bonded to the Ti2AlNb using the vacuum brazing approach. The microstructure of the joint is AlON/(Cu, Al)3Ti3O/Ag (s, s) +AlCu2Ti + Cu (s, s)/AlCu2Ti/TiCu/Ti2Cu/Ti2AlNb. The highest shear strength of the joint brazed with AgCuTi is obtained at 830 degrees C for 10 min, which was 27.6 MPa. The residual stress generated from the CTE mismatch between AlON and Ti2AlNb is alleviated by adding negative thermal expansion LiAlSiO4 into the AgCuTi brazing filler. The residual stress in the joint is measured via Raman spectra and the addition of LiAlSiO4 could lower the residual stress by up to 12.9%. The highest shear strength of 96.1 MPa could be reached at 860 degrees C for 10 min with 2 wt% LiAlSiO4 + AgCuTi as the brazing filler, which is ~248% higher than the joint obtained with AgCuTi brazing filler.
What problem does this paper attempt to address?