Abstract:It is still a great challenge to fabricate dense solid electrolyte with high ionic conductivity using a facile and low-cost method for all solid-state rechargeable battery. In this context, a cold sintering process (CSP) is employed to prepare the ceramic solid electrolytes at an extremely low temperature of 120 degrees C, significantly suppressing the Li loss and impurity formation by traditionally high-temperature sintering. The low temperature prepared Li1.5Al0.5Ge1.5(PO4)(3) (LAGP)-LiClO4 (10.0 wt%) composite electrolyte exhibits a high ionic conductivity of 6.35 x 10(-5) S/cm, low activation energy of 0.26 eV and high relative densities of 90%. The Li | CSP LAGP-LiClO4 (10.0 wt%) | Li symmetric cell delivers a cycling time retention of over 350 h with a stabilized voltage overpotential at a current density of 0.2 mA/cm(2). Moreover, the high Coulombic efficiency of 99.97% and capacity retention of 150 mAh/g are achieved after 130 cycles at 0.1C in Li | CSP LAGP-LiClO4 (10.0 wt%) | LiFePO4 solid cells. These good electrochemical performances are originated from the well-constructed solid electrolyte-electrode interfaces, where the electrochemically active interface demonstrates the powerful self-stabilization function to maintain the tight interface connection as well as the continuous Li ion transport. The CSP method sheds new light on the fabrication of solid electrolytes at a low temperature and inexpensive way, hence provides a rewarding avenue to fabricate better solid-state batteries and other electrochemical devices. (c) 2021 Elsevier Ltd. All rights reserved.
What problem does this paper attempt to address?