Efficient Chemical Prelithiation with Modificatory Li+ Solvation Structure Enabling Spatially Homogeneous SEI toward High Performance SiOx Anodeâ€
Ruoyang Wang,Yuqing Wu,Yifan Niu,Qing Yang,Haoyu Li,Yang Song,Benhe Zhong,Liwen Yang,Ting Chen,Zhenguo Wu,Xiaodong Guo
DOI: https://doi.org/10.1002/cjoc.202400226
IF: 5.56
2024-05-01
Chinese Journal of Chemistry
Abstract:Weak solvent‐driven prelithiation achieves efficient and uniform prelithiation effects, yielding LiF‐rich, homogeneous, and stable solid electrolyte interphases without any alterations to the SiOx or electrolyte. The prelithiation process splits the SEI film formation process into two parts: pre‐decomposition of the organic component and post‐filling of the inorganic component, which broadens the idea of SEI film modulation strategy. Comprehensive Summary Chemical prelithiation is widely proven to be an effective strategy to address the low initial coulombic efficiency (ICE) of promising SiOx anode. Though the reagent composition has been widely explored, the Li+ solvation structure, which practically plays the cornerstone role in the prelithiation ability, rate, uniformility, has rarely been explored. A novel environmentally‐friendly reagent with weak solvent cyclopentyl methyl ether (CPME) is proposed that enables both improved ICE and spatial homogeneous solid electrolyte interphase (SEI). And the prelithiation behavior and mechanism were explored focused on the Li+ solvation structure. Both theoretical investigation and spectroscopic results suggest that weak solvent feature of CPME reduces the solvent coordination number and decreases the Li+ desolvation energy. The optimized Li+ solvation structure enables high‐efficiency prelithiation that ensures the horizontal homogenization and mechanical properties of SEI. Moreover, the accompanied CPME molecules preferentially occupy positions in initial SEI, reducing the likelihood of LiPF6 decomposition and promoting longitudinal homogenization of SEI. Consequently, the efficient and homogenous prelithiation enables impressive ICE of 109.52% and improved cycling performance with 80.77% retained after 300 cycles via just 5 min soaking. Furthermore, the full cells with LiNi0.83Co0.12Mn0.05O2 (NCM831205) cathode display an enhancement in the energy density of 179.74% and up to 648.35 Wh·kg–1.
chemistry, multidisciplinary