Fabrication of Ti<sub>66</sub>V<sub>13</sub>Cu<sub>8</sub>Ni<sub>6.8</sub>Al<sub>6.2</sub> Bulk Composites with High Strength by Spark Plasma Sintering and Crystallization of Amorphous Phase

Xue Mei Wu,Wei Ping Chen,Chao Yang,Sheng Guan Qu,Yat Li
DOI: https://doi.org/10.4028/www.scientific.net/amr.284-286.25
2011-01-01
Advanced Materials Research
Abstract:Ti 66 V 13 Cu 8 Ni 6.8 Al6.2 bulk composites with high strength were fabricated by spark plasma sintering of amorphous Ti 66 V 13 Cu 8 Ni 6.8 Al 6.2 powder synthesized by mechanical alloying. X-ray diffraction (XRD), differential scanning calorimeter (DSC), scanning electron microscopy (SEM), and transmission electron microscopy (TEM) were employed to investigate the synthesized amorphous powder and the fabricated composites. Results show that the supercooled liquid region ΔT x and the crystallization enthalpy D H x of the synthesized amorphous powder decrease, in relative with amorphous Ti 66 Nb 13 Cu 8 Ni 6.8 Al 6.2 powder, indicating that the thermal stability and glass forming ability of the synthesized amorphous powders decreases with vanadium element substituted for niobium element. And particle size of the synthesized amorphous powder also decreases. In addition, the fabricated alloys also consist of body-centered cubic β-Ti (V) and face-centered cubic (Cu, Ni)-Ti 2 regions, similar to Ti 66 Nb 13 Cu 8 Ni 6.8 Al 6.2 bulk alloys. The alloys exhibit a high fracture strength around 1966 MPa but limited plasticity.
What problem does this paper attempt to address?