蠕虫状孔道介孔SiO 2 的合成及其固定化漆酶的活性

张剑波,杨宇翔,田美娟,邓常健,曹磊,袁宏明
DOI: https://doi.org/10.6023/a12100836
2013-01-01
Acta Chimica Sinica
Abstract:Mesoporous silica with worm-like pore channels was synthesized using mixed P123 (polyethyleneox- ide-polypropylene oxide-polyethylene oxide triblock copolymer EO20PO70EO20) and ionic cosurfactant {CTAB, SDS or N-myristoyl-D-alanine (C14-D-A)} as a structure-directing agent, and the pore-expanding effect of different amount of PEG-400 on the worm-like pore channels was studied. The synthesized products were characterized using X-ray diffraction, scanning electron microscopy, transmission electron microscopy, and nitrogen sorption analysis. Moreover, the worm-like pore-expanded mesoporous silica was extracted with solvent, and the obtained quaternary ammonium functionalized mesoporous silica with different pore size was applied to immobilize laccase respectively. The stability of immobilized lac- case, the optimum pH value acquired and reusability for the degradation of 2,4-DCP were also studied. Through comparative studies, it is found that, matching of sizes between the enzyme molecule and the pore diameter of the mesoporous silica, is essential for specific activity of immobilized laccase and degradation efficiency of 2,4-DCP by immobilized laccase. Keywords worm-like mesoporous silica; pore-expanding, 2,4-DCP; degradation efficiency; reusability
What problem does this paper attempt to address?