Abstract:Series of ferroelectric glass-ceramic samples of Sr0.5Ba0.5Nb2O6 were synthesized by melting method. Firstly, analytical reagents were melted for 30 minutes at 1440°C after being grinded evenly according to a certain molar ratio, then annealed for 10 hours from 550°C to room temperature, finally it was sustained for 4 hours at constant temperature about 700°C. The hardness and transmittance parameters of SBN glass-ceramic were tested. Results indicated the sample had the best property when the amount of Nb2O5 was 10mol%, whose hardness reached 506 kg/mm2, and spectral transmittance was higher than 35% . XRD spectra of this sample indicated this SBN glass-ceramics contained a large number of Sr0.5Ba0.5Nb2O6 crystalline phase and a small amount of Sr0.3Ba0.7Nb2O6 phase. The particle size was about 50 nm.
What problem does this paper attempt to address?