Effect of Rolling Temperature and Subsequence Ageing on the Mechanical Properties and Microstructure Evolution of an Al-Cu-Li Alloy

Lin Wang,Charlie Kong,Puneet Tandon,Alexander Pesin,Denis Pustovoytov,Hailiang Yu
DOI: https://doi.org/10.3390/met11060853
IF: 2.695
2021-01-01
Metals
Abstract:The mechanical properties and microstructure evolution of an Al-Cu-Li alloy sheet processed via hot rolling (HR) (at 400 degrees C and 500 degrees C) or cryorolling (CR) (at -100 degrees C and -190 degrees C) and subsequence aging at 160 degrees C for 10 h were investigated. Before aging, the highest ultimate tensile strength of 502 MPa was achieved when the sheets were cryorolled at -190 degrees C, while the better ultimate tensile strength of 476 MPa and the best elongation rate of 11.1% was achieved simultaneously when the sheets were cryorolled at -100 degrees C. The refined grains and numerous uniform deformation-induced dislocations microstructures were responsible for the improved strength and enhanced ductility of the cryorolled sheets compared to that of the alloy processed by hot rolling with a low dislocation density zone (LDDZ) and high dislocation density zone (HDDZ). After aging at 160 degrees C for 10 h, the ultimate tensile strength further improved resulted from the greater precipitation strengthening, and the increased precipitates provided greater resistance to dislocations movement resulting in the increased ductility although the dislocation density decreased. The uniform dislocation microstructures in the cryorolled sheets provide numerous nucleation sites for the precipitates, leading to higher strength after aging.
What problem does this paper attempt to address?