Sodium poisoning mechanism and regeneration of commercial De-NOx SCR catalysts

GAO Fengyu,TANG Xiaolong,YI Honghong,ZHAO Shunzheng,LI Dong,MA Ding,ZHANG Tongtong
DOI: https://doi.org/10.11817/j.issn.1672-7207.2015.06.052
2015-01-01
Abstract:Sodium poisoning of commercial De-NOx SCR catalysts (V2O5-WO3/TiO2) and the regeneration of deactivated catalysts by water and 0.5 mol/L H2SO4 were studied under simulated condition in laboratory. The physicochemical properties of catalysts were characterized by SEM, BET and XPS measurements, the reaction and deactivation mechanism of V2O5/TiO2 were also analyzed and discussed. The results indicate that catalysts are poisoned seriously with low-capacity Na2O, the catalytic activity of deactivated catalysts are recovered at varying degrees by washing with water and sulfuric acid, and the regeneration effect of washing with sulfuric acid is better than that of washing with water. Deposition of sodium salts particles and blocking of the pores and channels cause the physical poisoning of catalysts, and the main reason of chemical poisoning is attributed to the reaction of Na and V—OH to V—O—Na on the Br?nsted acid sites, which results in the changes of the chemical environment of metallic oxide on the surface of catalysts, thus blocking the spread of NO and NH3 to the inner of catalysts. The results also indicate that the denitration performance of SCR catalysts has certain positive correlation with the contents of chemical adsorbed oxygen and the ratio ofw(V4+)/w(V5+) on the surface of catalysts.
What problem does this paper attempt to address?