Experimental Study on Low-Temperature Mechanical Properties of S30408 Welded Joints

DING Hui-ming,WU Ying-zhe,ZHENG Jin-yang,CHEN Zhao-hui,YIN Li-jun
DOI: https://doi.org/10.3785/j.issn.1008-973x.2018.02.002
2018-01-01
Abstract:Tensile and impact tests at-196 ~ 20 ℃ were conducted out to obtain the low-temperature tensile properties and impact toughness of the S30408 base metal and welded joint.The experimental results show that the yield strength and tensile strength of both base metal and welded joint significantly increase with temperature decreasing due to the cryogenic strengthening effect.The Charpy absorbed energy and lateral expansion tend to degrade when temperature decreases.The welding zone has the worst impact toughness because it contains the largest amount of the ferrite content.The reduction of the impact toughness in the welding zone is related to the decreasing in the crack propagation resistance at cryogenic temperatures.The inhomogeneous ferrite distribution in the welded joint leads to non-uniform micromechanical properties which causes a plastic constraint on the deformation,and consequently results into a weak ultimate bearing capacity of the welded joint.
What problem does this paper attempt to address?