Abstract:Nano-LiMn_2O_4 spinel oxides has been prepared successfully by roasting precursor in the air atmosphere, while precursor was obtained by sol-gel techniques, with lithium nitrate and manganese nitrate as original material and citric acid as complexant. The thermal decomposition behavior of the precursor has been examined with the method of DTA-TG. The structure and purity of LiMn_2O_4 powder have been analyzed by means of XRD. The morphology of it also has been observed and grain size has been measured by SEM. The mean valency of manganese in LiMn_2O_4 has been determined by redox titration method. Results show that there're some obvious spinel structure of LiMn_2O_4 at 300 ℃. And the quality of LiMn_2O_4 can be remarkably improved after being pretreated at 300 ℃. The grain size and lattice constant tend to increase with the increase of temperature. After pretreatment, LiMn_2O_4 is in the form of sphericit, distributing evenly with the average grain size of 30 nm. The mean valency of manganese is 3.498, which is very close to the theoretical value.
What problem does this paper attempt to address?