Strain-induced precipitation behavior of new Fe-Cr-Ni heat-resistant alloy

ZHANG Pan-pan,CHENG Xiao-nong,LUO Rui,LIU Tian,GAO Tian-ming
DOI: https://doi.org/10.13228/j.boyuan.issn1001-0963.20180142
2019-01-01
Abstract:The isothermal strain-induced precipitation behavior of Fe-Cr-Ni heat-resistant alloy at temperature of600, 650, 700, and 750℃and compression of 0.4on a Gleeble-3500thermal mechanical simulator was studied by stress relaxation method.The experimental results show that the PTT curve of the material is a typical C curve, and the fastest precipitation temperature is about 650℃.There are three kinds of precipitates in austenite of this material, M23C6, NbC and Laves-Fe2Nb, and nanometer NbC is the main precipitation strengthening phase.