Microstructure and crystallization behaviour of laser welding FeSiB amorphous ribbon joint

GONG Yu-bing,WANG Shan-lin,LI Hong-xiang,ZHANG Zi-yang,CHEN Yu-hua
DOI: https://doi.org/10.19476/j.ysxb.1004.0609.2017.05.007
2017-01-01
The Chinese Journal of Nonferrous Metals
Abstract:FeSiB amorphous ribbons were successfully pulse laser lap welded, and the crystallization behavior in the weld was investigated in heat treatment. The effects of pulse power on weld formation, microstructure and tensile properties were studied, and the crystallization process of amorphous ribbon was analyzed by testing technologies. The results show that the weld surface is rough and the weld width is narrow when the power is below 4.8 W. However, some microcracks are formed on the weld surface with power exceeding 9.6 W. When the power is 7.2 W, the weld quality is best without welding defects. With the increase of pulse power, the tensile strength of the joint first increases and then decreases, the highest tensile strength reaches to 410 MPa. The failure of the joints is a cleavage fracture. Moreover, the microstructure in the joint is mainly composed of amorphous phase, dendrites, crystalline phase with white particle shape. An obvious crystallization process occurs during welding, where the α-Fe(Si) phase is firstly precipitated, and then the Fe2B phase is formed.
What problem does this paper attempt to address?