Enhanced Hydrometallurgical Pretreatment of Micro-disseminated Gold Ore

Dianqi YANG,Yun TANG,Lijing TANG,Jue WANG,Hongxin WANG
DOI: https://doi.org/10.3969/j.issn.1004-0676.2017.04.009
2017-01-01
Abstract:The effects of leaching conditions on gold recovery from a micro-disseminated gold ore were studied by following a non-cyanide leaching procedure with two-stage impregnation during inflation. The results showed the gold leaching rate can be increased by air inflation in 2 stages of oxidation and alkali pretreatment. After oxidation pretreatment for 2 hours, sodium hydroxide (20 kg/t) was added for ensuing alkali leaching pretreatment for 4 hours, and then the calcium oxide (40 kg/t) was added to replace the sodium hydroxide. Finally the TY-3 leaching agent (8 kg/t) was used to leach for 4 hours. An overall gold leaching rate of up to 87.21% was achieved. Phase analysis, SEM and X-ray energy spectrum of the resulting residues showed that the gold in silicate and carbonate could be effectively leached out. The quartz and pyrite surface in leaching residues had been corroded, and also part of pyrite was oxidized.
What problem does this paper attempt to address?