Effect of normalizing on magnetic properties of high-manganese 50W470 non-oriented silicon steel

Fan Yang,Yanxia Hua,Chen Zhang,Shengtao Qiu
DOI: https://doi.org/10.13251/j.issn.0254-6051.2015.11.038
2015-01-01
Abstract:Effects of normalizing treatment at 900-1000 ℃ on microstructure, texture and magnetic properties of high-manganese 50W470 non-oriented silicon steel were investigated .The results show that the magnetic induction increases with the increase of normalizing temperature, and the lowest iron loss appears at 975 ℃.The grain size of hot rolled plate after normalizing increases with the increase of normalizing temperature , while the corresponding grain size of final product after cold rolling and annealing increases first and then decreases ( the maximum at 975 ℃) .{100} texture and Gauss texture can be obtained in the final products of silicon steel plate after normalizing at 975 ℃for 5 min, such can improve the magnetic properties .The optimal normalizing process of high-manganese 50 W470 non-oriented silicon steel is normalizing at 975 ℃ for 5 min.Normalizing treatment can improve the microstructure and texture of high-manganese non-oriented electrical steel , and finally improve the electromagnetic properties of it .
What problem does this paper attempt to address?