Effect of heat treatment on microstructure and mechanical properties of as-cast Mg-5Y-2Nd-3Sm-0.5Zr alloy

GUI Yun-wei,LI Quan-an,ZHANG Xing-yuan,CHEN Xiao-ya,WANG Song-bo,OUYANG Yun-fei,DONG Yao-gang
DOI: https://doi.org/10.13289/j.issn.1009-6264.2017-0556
2018-01-01
Abstract:Effects of solid solution and aging treatment on microstructure and mechanical properties of as-cast Mg-5Y-2Nd-3Sm-0.5Zr alloy were investigated by means of optical microscope (OM), scanning electron microscopy (SEM) equipped with energy dispersive spectroscopy(EDS), X-ray diffraction (XRD), transmission electron microscopy (TEM), Vickers hardness test and universal mechanical tensile test. The results show that the microstructure of the as-cast alloy is mainly composed of α-Mg matrix, Mg24Y5, Mg41 Nd5 and Mg41 Sm5 phases. After solid solution treatment, the coarse precipitated phases in the as-cast alloy are dissolved into the α-Mg matrix, and a new nanoscale precipitated phase is observed in the alloy after aging treatment. The optimum heat treatment for the as-cast alloy is solid solution at 525 ℃ for 10 h then aging at 225 ℃ for 12 h. After the optimum heat treatment, the alloy has the best mechanical properties, and its hardness, tensile strength, yield strength and elongation are 124.8 HV, 296.9 Mpa, 255.4 Mpa and 5.78%, respectively.
What problem does this paper attempt to address?