Effects of Heat Treatment on Microstructure and Mechanical Properties of Mg-8Gd-3Y-0.5Zr (wt.%) Alloy Fabricated by Semi-Continuous Casting

Jun Yang,Qu-dong Wang,Huan Wang
2015-01-01
Abstract:The microstucture, mechanical properties and fracture behaviors of semi-continuous cast Mg-8Gd-3Y-0.5Zr (wt.%, GW83K) alloy after different heat treatments were investigated. Almost all the eutectic compounds were dissolved into the matrix and there was no evident grain growth after optimum solution treatment at 500 degrees C for 4 h. Further ageing at low temperatures led to significant precipitation hardening, which strengthened the alloy. Peak-aged at 200 degrees C, the alloy had the highest ultimate tensile strength (UTS) and lowest elongation at 395 MPa and 2.8%, respectively. When aged at 225 degrees C for 15 h, the alloy exhibited prominent mechanical performance with UTS and elongation of 363 MPa and 5.8 %, respectively. With regard to microstructure and tensile properties, the processes of 500 degrees C, 4 h + 225 degrees C, 15 h are selected as the optimal heat treatment conditions. The alloy under different conditions shows different fracture behaviors: in the as-cast alloy, a quasi-cleavage pattern is observed; after solution treatment, the alloy exhibits a trans-granular quasi-cleavage fracture; after being peak-aged at 200 degrees C and 225 degrees C, the fracture mode is a mixed mode of trans-granular and intergranular fracture, in which the inter-granular mode is dominant in the alloy peak-aged at 200 degrees C.
What problem does this paper attempt to address?