Effect of Electrolytic Parameters on Surface Morphology and Microstructure of 2A12 Al Alloy

Cheng ZHU,Kaiyue LI,Shiliang WANG,Qingfeng ZHU,Zhihao ZHAO
DOI: https://doi.org/10.14158/j.cnki.1001-3814.2018.14.034
2018-01-01
Abstract:The effects of anode voltage, current and polishing time on the surface morphology and microstructure of2 A12 aluminum alloy were studied. The results show that when the voltage is less than 23.7 V, the metal surface dissolves slowly, without forming a passivation film, not up to the requirements of polishing; when the voltage is above 30.8 V, the current density is larger, the corrosion rate increases, resulting in the corrosion of part dendrites phase of the alloy; when the voltage is 23.7-30.8 V, the stage is an effective electropolishing stage. With the polishing time increasing from 0 to 30 s, the current decreases first and then increases continuously under the voltage of 30 V. When the electropolishing time is 5 s, the current is the smallest, the electropolishing effect is the best, and the surface of the sample is smooth and light, and the microstructure is clear.
What problem does this paper attempt to address?