Study on the Yield Improvement of Handle Spray Products

Chao Chen,Yong Li,Lu Yang,Yanxiu Zhou,Yiye Yi
DOI: https://doi.org/10.3969/j.issn.1001-3849.2018.05.008
2018-01-01
Abstract:urface pitting defects exist on the customer's hand spray products,lead to the yield of only 29.41%.In view of this problem,the specific reasons for the defects of the product were analyzed based on the productive practice,and the improvement measures of product quality were researched.The results showed that defect of the product was mainly caused by particles,slag and grain on the surface of the substrate.Product percent of pass could be stabilized over 90% through abrasive blasting,alkaline etching,second-spray and repair using chemical reparation agent.