Phosphate removal by using magnesium oxide/construction waste of subway composite ceramsite

Hai-bin LI,Fa-zhi XIE,Han XUAN,Dan-dan SHENG,Ting-ting HU,Xue-chun WANG,Zhi-yong XIE
DOI: https://doi.org/10.16581/j.cnki.issn1671-3206.2015.09.002
2015-01-01
Abstract:Using solid waste residue of subway construction as the main raw material,mixing with magnesi-um oxide,a novel composite ceramsite was prepared. Sintering temperature,content of magnesium oxide, effect of adsorption pH,temperature and contact time were investigated. The optimal preparation of the com-posite ceramsite obtained at 300℃ after preheating 25 min and then 20 min of sintered at 700℃,which the content of magnesium oxide was 20%. The optimum of adsorption was pH 6. 0. Sorption capacity increased with increasing the sorption temperature, and the maximum sorption capacity can reach 3 811. 6 mg/kg when the initial temperature was 80 ℃. The adsorption kinetics was reasonable fast,and sorption equilibri-um can reach within 2 h,and the Lagergren pseudo-second-order kinetics can fit the data well.
What problem does this paper attempt to address?