Abstract:In the production of tin, much Sn-Cu bearing residue is yielded, and it is an important secondary resource for Sn and Cu recovery but has the disadvantages of a low metal recovery rate and low-concentration SO2 pollution. In this study, alkaline pressure oxidative leaching (APOL) was proposed to dispose of the Sn-Cu bearing residue. Tin was first dissolved as sodium stannate into the filtrate and used for SnO2 synthesis via a hydrothermal process, while copper sulfides were oxidized to copper oxide, and used for CuSO4 center dot 5H(2)O preparation via acid leaching evaporative crystallization. Under the optimized leaching conditions of APOL, the leaching efficiencies of Sn, As, and S approached 93.42%, 98.82%, and 97.99%, while the leaching efficiency of copper was only 1.60%, which results in the efficient extraction of tin, desulfurization, dearsenification, and separation of tin and copper. The product SnO2 had a purity higher than 99.86%, a morphology of irregular shape, and a mean size of 2.68 mu m. Meanwhile, the purity of prepared CuSO4 center dot 5H(2)O reached 99.98% with a morphology of irregular rods. Both valuable metals are economically and efficiently recycled by this environmentally friendly method.