The Biocompatibility of Nitinol in Guinea pigs’ Acoustic Vesicle
Zhang Yuanyuan,Xiao Zian,Li Zhou,Xu Guofu,Huang Boyun
DOI: https://doi.org/10.3969/j.issn.1006-7299.2010.03.003
2010-01-01
Abstract:Objective To explore the biocompatibility of Nitinol(NiTi) after being implanted in guinea pigs' acoustic vesicle.Methods 50 healthy guinea pigs with normal hearing were used in this study.One ear of each guinea pig was selected as the experimental group randomly (NiTi implanted in the acoustic vesicle,50 ears).The lefte ears of the guinea pigs were divided into control group I (Ti implanted group,25 ears) and control group II (opened acoustic vesicle without implanting,25 ears) equally.5 guinea pigs in control I and 5 guinea pigs in control II were executed at 7th,14th,28th,56th,112th day after operation,respectively.Whether there was granulation hyperplasia around the implanted materials,and corrosion spot and colour changing occurred on the surface of the implanted materials were observed.Then,the surface topography and the elemental composition of the neonatal tissues on the surface of the materials were observed and analyzed by the Field Emission Scanning Electron Microscope (FEI Co,USA) and the Energy Dispersive Analysis (EDAX Co,USA),respectively.Results There was neonatal bone-like tissue on the surfaces of NiTi implant but no inflammatory granulation tissue around them,and no corrosion spot and colour changing occurred on the surface of the implanted NiTi and in the Ti implant.Neonatal tissue scatterred on the surface of NiTi and Ti at 7th day,gradually interweaved into mesh from 14th to 56th day and finally developed to plate at 112th day after operation.The neonatal bone on NiTi contained very small amount of Ni and Ti elements and that on Ti implant with very slight of Ti element.Conclusion The bone-formation reaction and biocompatibility of NiTi in the acoustic vesicle are outstanding,but with very small amount of Ni releasing from NiTi and its biological toxicity should be further studied.