Plastic and Elastic Strains in Poplar Wood under High-Pressure Densification

A. Li,K. Yan,H. S. Ramaswamy,S. Zhu,Y. Yu
DOI: https://doi.org/10.13031/trans.13869
2020-01-01
Transactions of the ASABE
Abstract:Highlights High-pressure densification (HPD) resulted in more than 100% increase in the density of poplar wood. Density of wood during HPD treatment was up to 300% and 100% higher than observed before and after HPD. A method was developed to measure elastic recovery in the radial and tangential directions under HPD. Abstract . Plastic and elastic strains of poplar wood in the radial and tangential directions were investigated after high-pressure densification (HPD) using a special method that detected the elastic strain. There was a large difference in plastic and elastic strains obtained in compressed wood between the radial and tangential directions. The maximum total strain in the radial and tangential directions reached 26.9% and 66.9%, respectively, when compressed at 150 MPa for 300 s. Longer holding time (300 s) increased the plastic strain, by reducing the elastic strain, when the applied pressure was lower than 60 MPa. In addition, a large difference in compressed wood density prevailed when still under pressure as compared with the density measured after the pressure treatment, and both were nearly 1 to 3 times higher than the density of fresh wood. Further, the maximum density observed under pressure was related to the maximum reported density of dry crystalline cellulose plus the entrapped moisture. The mechanical properties of densified wood were also investigated and found to depend on the pressure treatment conditions. Keywords: Elastic strain, High-pressure densification, Mechanical properties, Plastic strain, Wood density.
What problem does this paper attempt to address?