Hydrogen-induced Delayed Fracture of a 1180 MPa Martensitic Advanced High-Strength Steel under U-bend Loading

Huixing Li,Jeffrey Venezuela,Qingjun Zhou,Vladimir Luzin,Ming Yan,Zhiming Shi,Ruth Knibbe,Mingxing Zhang,Futao Dong,Matthew S. Dargusch,Andrej Atrens
DOI: https://doi.org/10.1016/j.mtcomm.2020.101887
IF: 3.8
2020-01-01
Materials Today Communications
Abstract:Hydrogen-induced delayed failure (HIDF) of an 1180 MPa martensitic advanced high-strength steel (MS-AHSS) was studied using U-bend tests. HIDF susceptibility was increased by increasing stress, plastic strain and hydrogen content. Fracture initiated in the region of high tensile stress at the apex of the U-bend specimen. Hydrogen-induced fracture propagated in two stages, coinciding with the two stress regions of the specimen. The hydrogen content of the U-bend specimen increased with plastic strain and hydrogen fugacity. Delayed fracture is possible for specimens (and components) that contain substantial damage due to plastic strain and are subjected to a substantial stress.
What problem does this paper attempt to address?