Influence of Hydrogen on the S–N Fatigue of DP1180 Advanced High-Strength Steel

Huixing Li,Futao Dong,Qingjun Zhou,Zhiming Shi,Jeffrey Venezuela,Ming Yan,Ruth Knibbe,Mingxing Zhang,Andrej Atrens
DOI: https://doi.org/10.1016/j.corsci.2022.110465
IF: 7.72
2022-01-01
Corrosion Science
Abstract:We studied the load-controlled fatigue behaviour (at a stress ratio R = 0.1, 1 Hz, using smooth flat-sheet specimens) in air and with hydrogen (electrochemically charged at a current density of 16 mA cm(-2) in 0.1 M NaOH) for a 1180 MPa dual-phase advanced high-strength steel. There was no significant difference between the fatigue lives with hydrogen and in air, even though there was a clear influence of hydrogen on the fatigue fractography. The hydrogen diffusion coefficient (0.8 x10(-6) cm2 s(-1)) and a hydrogen content of 1.0 mu g g(-1) were evaluated using hydrogen permeation experiments. A rougher surface produced a shorter fatigue life.