Evolution of Microstructure, Residual Stress, and Tensile Properties of Additively Manufactured Stainless Steel under Heat Treatments

Zhang Xinchang,McMurtrey Michael D.,Wang Liang,O’Brien Robert C.,Texas A&M University,Wang Yun,Scott Randall,Ren Yang,Sun Cheng
DOI: https://doi.org/10.1007/s11837-020-04433-9
2020-01-01
JOM
Abstract:This study investigated the microstructure, residual stress, and tensile properties of directed energy deposited stainless steel 316L (SS316L) under thermal annealing. Microstructure characterization shows the as-printed sample has laser-generated patterns where dendritic structure is observed at the edge of the patterns and cellular structure dominates the interior region. The thermal annealing at 983 and 1093°C effectively removes the dendritic/cellular structures. Synchrotron x-ray diffraction reveals that the as-printed SS316L exhibits compressive residual stress of − 197.4 MPa, which is greatly relieved to − 53.8 MPa after annealing at 1093°C. The room temperature tensile testing indicates that the yield strength and ultimate tensile strength drop from 378 MPa and 502 MPa in the as-printed sample to 258 MPa and 446 MPa in the annealed samples (1093°C), respectively. Our study provides insights into the relationship among microstructure, residual stress, and tensile properties of laser additive manufactured SS316L.
What problem does this paper attempt to address?