Hydrometallurgical Stepwise Recovery of Copper and Zinc from Smelting Slag of Waste Brass in Ammonium Chloride Solution

Zhimei Xia,Xiaosa Zhang,Xinglong Huang,Shenghai Yang,Yongming Chen,Longgang Ye
DOI: https://doi.org/10.1016/j.hydromet.2020.105475
IF: 4.217
2020-01-01
Hydrometallurgy
Abstract:A new process for recycling zinc and copper from the smelting slag of waste brass was investigated in this study. The zinc and copper present in the smelting slag were dissolved in a ZnCl2-NH4Cl solution system. To recycle copper, the lixivium was purified by a novel method termed as electrochemistry and chemistry synergetic (ECS) purification. After deep purification of the ECS-treated lixivium by zinc powder cementation, zinc in the lixivium was extracted by electrowinning to obtain a zinc plate. The effects of the leaching temperature, reaction time, and liquid-solid ratio on the extraction percentages of zinc and copper were examined. The results revealed that the extraction percentages of zinc and copper were 88.37% and 90.85%, respectively, at a leaching temperature of 95 degrees C, reaction time of 90 min, and liquid-solid ratio of 8:1 mL/g. Further, effects of the current density, temperature, and reaction time on the recovery ratio of copper by ECS method were examined. The results revealed that 98.51% of copper could be extracted from the lixivium and that the purity of the extracted copper was 96.7% at a temperature of 70 degrees C and cathode current density of 75 A/m(2) after a reaction for 4 h. In the deep purification process, 0.3 g/L zinc powder was used to completely remove impurities from the ECS-treated lixivium. In the zinc electrowinning process, a current efficiency of 95.79% was achieved at 70 degrees C and 400 A/m(2); the purity of the obtained zinc product was greater than 99.95%, and the direct energy consumption was 2966.59 kW.h/t-Zn.
What problem does this paper attempt to address?