Superplasticity and Sinter-Forging of Fine-Grained Si3N4-Si2N2O Composite

JT Luo,KF Zhang,GF Wang,WB Han
DOI: https://doi.org/10.4028/www.scientific.net/msf.475-479.2987
2005-01-01
Materials Science Forum
Abstract:The Si3N4- Si2N2O composites are fabricated with amorphous nano-sized silicon nitride powders by the liquid phase sintering(LPS) method in this article. XRD analysis shows that the sintered body consists of β-Si3N4 and Si2N2O. SEM experiment conforms that the average grain size of sintered body is less than 300nm. The superplastic deep-drawing forming can be proceed at a low temperature of 1550°C with a forming velocity of 0.2mm/min. There are only a few small sintered defects before forming, but there are a lot of cavity groups after forming. Cavitation failure occurs by nucleation, growth and interlinkage of cavities. The complex-shape gears can be formed by a sinter-forging technology when the sintering temperature is 1600°C and the superplastic forging temperature is 1550°C.