Direct-white-emitting Phosphor SrAl2O4: Eu2+/3+ with Colour-Tunable Photoluminescence by Variation of Europium Activator Valence

Ziyao Wang,Yangai Liu,Zhaohui Huang,Minghao Fang,Xiaowen Wu
DOI: https://doi.org/10.1088/2053-1591/aad726
IF: 2.025
2018-01-01
Materials Research Express
Abstract:Eu2+ and Eu3+ co-doped phosphors SrAl2O4: Eu were synthesized in air via conventional solid-state reaction. The composition and valance state of doped ions were examined and verified by x-ray photoelectron spectra (XPS), diffuse reflection spectra and photoluminescence (PL)/photoluminescence excitation (PLE) spectra. Under ultraviolet (UV) excitation, the broad emission peaking at 519 nm was assigned to the 4f65d–4f7 transition of Eu2+, and the series of narrow bands peaking at 619 nm originated from the 4f–4f transition of Eu3+ ions. The self-reduction processing of Eu3+ could be controlled by the variation of the Eu3+ doping concentration, annealing temperature and holding time, and the emission colour of synthesized phosphors could be regulated from yellowish green to white. The optimized doping concentration of Eu3+ was 1 mol%, and the annealing temperature and holding time were 1350 °C and 3 h, respectively. Accordingly, the phosphor emitted white light under the excitation of 365 nm with the CIE coordinates (0.3312, 0.3578) and colour temperature 5562 K.
What problem does this paper attempt to address?