Preparation method Fe/ZSM 5 catalyst for directly decomposing N2O

Can Li,Haian Xia,Keqiang Sun,Zhaochi Feng,Pinliang Ying
2009-01-01
Abstract:The invention relates to a method for preparing an Fe/ZSM-5 catalyst for directly decomposing N2O, which comprises the following steps: (a), roasting NH4-ZSM-5 zeolite molecular sieves at a temperature of between 500 and 600 DEG C for 2 to 6 hours, cooling and sealing the NH4-ZSM-5 zeolite molecular sieves, and moving the NH4-ZSM-5 zeolite molecular sieves into a drying cabinet; (b), mixing and grinding the zeolite molecular sieves treated in the step a and an iron salt precursor, raising the temperature to be between 300 and 400 DEG C in inert atmosphere, and maintaining the mixture for 1 to 2 hours, wherein the content of iron is 0.01 to 10 weight percent of the total weight of the zeolite molecular sieves and the iron salt precursor; (c), cooling the product in the step b, and hydrolyzing the product in vapor-containing inert atmosphere for 1 to 2 hours at a temperature of between 150 and 200 DEG C; and (d), roasting the product in the step c in oxygen atmosphere for 1 to 2 hours at a temperature of between 500 and 600 DEG C and at a temperature rise speed of between 1 and 8 DEG C per minute.
What problem does this paper attempt to address?