Synthesis and Characterization of Perfluorocyclobutyl Copoly(aryl ether)s Containing Biphenyl and Sulfonyl Moieties

Qian Liu,Yu-xue Yang,Shou-hai Zhang,Ren-dong Xue,Xi-gao Jian
DOI: https://doi.org/10.11777/j.issn1000-3004.2017.17211
2018-01-01
Acta Polymerica Sinica
Abstract:High temperature solution copolymerization of 4,4'-sulfonyl-bis(trifluorovinyloxy)biphenyl (DTS) and 4,4 '-bis(trifluorovinyloxy)biphenyl (DTB) were carried out in diphenyl ether as the solvent. A series of perfluorocyclobutyl copoly(aryl ether)s containing biphenyl and sulfonyl moieties (PFCB-S-BP) were prepared via thermal [2 pi + 2 pi] cycloaddition polymerization by controlling the ratio of DTS to DTB. PFCB-S-BP was synthesized when the ratio of DTS to DTB ranged from 3/7 to 7/3. Molecular weight and its distribution of PFCBS-BP were measured by gel permeation chromatography (GPC). The GPC curves showed a narrow and unimodal elution peak. The number-average molecular weight of PFCB-S-BP was larger than 1.4 x 10(4), with a narrow molecular weight distribution ranging from 1.4 to 1.6. The chemical structures was characterized by Fourier transform infrared spectroscopy Fourier transform infrared spectroscopy (FTIR), hydrogen nuclear magnetic resonance (H-1-NMR) and fluorine nuclear magnetic resonance (F-19-NMR). The characteristic signal of trifluorovinyl ether group of monomers at 1824 cm(-1) disappeared in Fourier transform infrared spectroscopy (FTIR) spectra of PFCB-S-BP and the strong perfluorocyclobutyl group characteristic peak at 957 cm(-1) appeared. The intensities of sulfonyl group characteristic absorption peaks at 1100 and 1315 cm(-1) increased with the increase in the ratio of DTS to DTB. From 1 H-NMR of PFCB-S-BP, the signal at 7.9 was assigned to the protons of benzene ring adjacent to sulfonyl group. The intensity of the signal increased with an increase in the ratio of DTS to DTB. For F-19-NMR of PFCB-S-BP, the multiple peaks ranging from -127 to -134 were ascribed to the cis- and trans-substituted PFCB rings. These results indicated that DTS copolymerized with DTB, and PFCB-S-BP copolymers were successfully synthesized. The thermal property and solubility of PFCB-S-BP were also tested. T-g of PFCB-S-BP increased slightly from 146 degrees C to 153 degrees C with an increase in the ratio of DTS to DTB from 3/7 to 7/3. The decomposition temperature for 5% weight loss of PFCB-S-BP was above 470 degrees C. These results showed that PFCB-S-BP exhibited high thermal stability and was soluble in common organic solvents such as N-methyl-2-pyrrolidinone, N,N-dimethylacetamide and chloroform.
What problem does this paper attempt to address?