Fabrication of SiC whisker reinforced laminated Si3N4/BN ceramics by spark plasma sintering

CW Li,Y Huang,CA Wang,K Tang,SQ Li
DOI: https://doi.org/10.3321/j.issn:1000-324X.2002.06.023
IF: 1.292
2002-01-01
Journal of Inorganic Materials
Abstract:SiC whisker reinforced laminated Si3N4/BN ceramics with additives Y2O3, Al2O3 and MgO were prepared by spark plasma sintering(SPS) in 13min of heating to 1650degreesC and 15min dwell time. The density of the samples densified by SPS was 3.18g/cm(3). Bending strength reached 600 MPa, and the work of fracture reached 3500 J/m(2). The arrangement of hard Si3N4 layer and soft BN layer, the pull-out and broken of SiC whisker were the main reason for improving toughness of this ceramic. XRD and SEM indicated SiC whisker, long rod like beta-Si3N4 and platelet like hex-BN were the main phase and SiC whisker, long rod like beta-Si3N4 had strong preferred orientation.