n metal oxides for high performance Naion battery cathodes †

Chao Luo,Alex Langrock,Xiulin Fan,Yujia Liang,Chunsheng Wang
2017-01-01
Abstract:The particle pulverization induced by volume change and the disproportionation reaction of Mn to Mn and electrolyte-soluble Mn are two major challenges for Na0.67MnO2 cathodes in Na-ion batteries. Herein, Ni and/or Fe doped Na0.67MnO2 was synthesized to suppress the particle pulverization and disproportionation reaction. The replacement of 33% Mn ions by Ni in Na0.67MnO2 can effectively reduce the particle pulverization and disproportionation of Mn, resulting in improved cycling stability at the cost of reduced capacity. To develop a high capacity and long cycle life cathode material, Ni in Na0.67Ni0.33Mn0.67O2 is further partially substituted by Fe to generate Na0.67Fe0.20Ni0.15Mn0.65O2, which retains 70% of its initial capacity after 900 cycles, corresponding to a very low capacity decay rate of 0.033% per cycle. To the best of our knowledge, the Na0.67Fe0.20Ni0.15Mn0.65O2 synthesized by ultrasonic spray pyrolysis (USP) represents one of the best cathode materials for Na-ion batteries to date. In addition, a thin layer (5 nm) of Al2O3 is deposited on the Na0.67MnO2 electrode by atomic layer deposition (ALD) to further reduce the dissolution of Mn ions and accommodate the volume change, which further extend the cycling stability of Na0.67MnO2 electrodes.
What problem does this paper attempt to address?