P2‐Type Na0.67Ni0.23Fe0.1Mn0.67O2 Cathode Material with Suppressed P2−O2 Phase Transition for Sodium‐Ion Batteries

Liang Xie,Weiqin Lu,Lanyan Li,Mingzhou Li,Xianyou Wang,Zhigao Luo
DOI: https://doi.org/10.1002/slct.202304590
2024-08-25
ChemistrySelect
Abstract:In this study, a modification strategy was proposed and implemented to replace the P2‐type Na0.67Ni0.33Mn0.67O2 with Fe. Fe substitution can suppress P2−O2 phase transition with a stable P2 phase during charging and discharging. Additionally, it also suppresses Na+/vacancy ordering, expands the slab‐spacing of the structure . Na0.67Ni0.33Mn0.67O2 (NNMO) is one of the most promising cathodes for Sodium‐ion batteries. However, due to undesired P2−O2 phase transition at high voltage during Na+ extraction, its cyclic stability and coulomb efficiency are greatly adversely affected. Herein, electrochemically active Fe3+ ions substituted Na0.67Ni0.23Fe0.1Mn0.67O2 samples were prepared by both sol‐gel method (NNFMO‐SG) and solid phase method (NNFMO‐SP). It has been found that Fe substitution can suppress P2−O2 phase transition with a stable P2 phase during charging and discharging. Additionally, it also suppresses Na+/vacancy ordering, expands the slab‐spacing of the structure and improves the reversibility of the redox of anions. Owing to the combined advantages, NNFMO‐SG material exhibits the enhanced rate capability (70.1 mAh/g at 1000 mA/g) and excellent cycling stability (75.3 % capacity retention after 100 cycles at 200 mA/g).
chemistry, multidisciplinary
What problem does this paper attempt to address?