Efficient extraction of slowly-released Cr(VI) from nano-sized ion channels in Cr(VI)-ettringite from reduced chromite ore processing residue
Weizhen Liu,Yao Song,Jing Li,Lan Ling,Chen Tian,Xueming Liu,Zhang Lin
DOI: https://doi.org/10.1039/d0en00074d
2020-01-01
Abstract:Residual unreacted Cr(VI) incorporated in ferrous-sulfate-reduced chromite ore processing residue (rCOPR) can be slowly released during deposition, posing a significant threat to the environment. Recent studies indicate that such Cr(VI) mainly exists within the nano-sized ion channels of ettringite, forming Cr(VI)-ettringite. Therefore, efficient extraction and recovery of the incorporated Cr(VI) from rCOPR, especially from Cr(VI)-ettringite, are urgently needed in order to eliminate the long-term hazardous effects of rCOPR. In this work, NaHCO3 was used to extract Cr(VI) from rCOPR with or without hydrothermal treatment, and the process under hydrothermal conditions (up to 120 degrees C) was able to nearly completely (>98%) extract Cr(VI). The results of X-ray diffraction, aberration-corrected scanning transmission electron microscopy, and X-ray absorption fine structure spectroscopy analyses were combined to elucidate the underlying extraction mechanisms. First, CO32- exchanged with CrO42- in the ion channels of Cr(VI)-ettringite, transforming ettringite into nano-CaCO3. This transformation effectively destroyed the ion-channel structure of Cr(VI)-ettringite, causing the release of incorporated CrO42-. However, in this stage, some CrO42- ions were still strongly adsorbed onto the nano-CaCO3, leading to the incomplete extraction of Cr(VI). Furthermore, the hydrothermal treatment was demonstrated to be essential to the acceleration of the nano-CaCO3 crystal growth to achieve the full Cr(VI) extraction. This novel strategy provides a viable approach to eliminate the pollution associated with the slow release of Cr(VI) from rCOPR in a fast and cost-effective manner. Environmental significance Contamination of soils and groundwater due to Cr(VI) in COPR and rCOPR constitutes a real environmental threat. With COPR, reduction and immobilization of Cr(VI) into the less toxic Cr(III), followed by deposition, have been widely used to remediate millions of tons of COPR worldwide with much success. However, the residual unreacted Cr(VI) incorporated in the mineral phases of rCOPR, which is mainly stored within the nano-sized ion channels of Cr(VI)-ettringite, can slowly leach out during deposition, causing a global concern for the long-term environmental risks of leaching. This work provides a feasible, low-cost approach to completely extract and recover incorporated Cr(VI) from rCOPR and eliminate the environment hazards associated with the long-term release of Cr(VI). This method is simple and feasible, and it can be easily scaled-up. The mechanisms involved in the process include ion exchange within the nano-sized ion channels of ettringite, the formation and growth of nano-CaCO3, and the associated separation of Cr(VI).