Freezing Site of Super-Cooled Water and Failure Mechanism of Cold Start of PEFC

Shangshang Wang,Ying Sun,Fusen Huang,Jianbo Zhang
DOI: https://doi.org/10.1149/2.0041913jes
IF: 3.9
2019-01-01
Journal of The Electrochemical Society
Abstract:The freezing site of super-cooled water and its effects on the triple-phase interface and pathway during PEFC cold start remain a subject of controversy. To address this deficiency, dynamic electrochemical characterizations, such as cyclic voltammetry (H 2 /N 2 ), galvanostatic (H 2 /Air) and potentiostatic EIS (H 2 /N 2 , at OCV and 0.2 V), are attempted during the isothermal sub-zero operation of a fuel cell from the start till the failure. The EIS data are fitted using transmission line models, revealing a significant rise in mass transfer resistance and rather constant ohmic, activation resistance and proton conductivity of catalyst layer. Consecutive CVs before, during and after the cell failure show no change. These results show that ice does not cover the surface of the catalysts, but rather blocks the pores of cathode catalyst layer, resulting in the suffocation of oxygen supply to the reaction sites. © The 2019. by ECS. This is an access article under the terms of the Creative Commons Attribution any Cold start capability is the key bottleneck restricting large-scale commercialization of fuel cell vehicles in cold regions. Fundamental understanding of ice formation and its effects on the triple-phase inter- face (TPI) and triple-phase pathway (TPP) in polymer electrolyte
What problem does this paper attempt to address?