Simultaneous Enhancement of Vascularization and Contact-Active Antibacterial Activity in Diopside-Based Ceramic Orbital Implants.

Jingyi Wang,Changjun Wang,Kai Jin,Xianyan Yang,Lingling Gao,Chunlei Yao,Xizhe Dai,Jinjing He,Changyou Gao,Juan Ye,Peng Li,Zhongru Gou
DOI: https://doi.org/10.1016/j.msec.2019.110036
2019-01-01
Materials Science and Engineering C
Abstract:Rapid vascularization and long-term antibacterial property are desirable characteristics of the next-generation implants in orbital reconstruction. In this study, the new diopside-based orbital implants were developed by direct ink writing of diopside (CaMgSi2O6; DIO) and low-melt bioactive glass (BG)-assisted sintering approaches. The mechanical tests showed that the addition 5% or 10% BG could readily enhance the compressive strength of the DIO porous bioceramics after sintering at 1150 degrees C. The Tris buffer immersion test in vitro indicated that the porous bioceramics exhibited appreciable mechanical stability and very limited mass loss (< 3.5%) after 8 weeks. The DIO/1OBG porous bioceramic sintered at 1150 degrees C or 1250 degrees C could promote appreciable angiogenesis response at the early stage (2-6 weeks) of implantation in the rabbit panniculus carnosus muscle models in vivo. It is interesting that the steam autoclaved bioceramics exhibited outstanding contact-active inhibition against Staphylococcus aureus and Pseudomonas aeruginosa, but as-sintered bioceramics showed no antibacterial effect. It is reasonable to consider that our strategy paves the way toward a simple and effective approach to fabricate the multifunctional tailormade implants for orbital implantation, thus accelerating the clinical translation of biomaterials research.
What problem does this paper attempt to address?