Extracting Antimony from High Arsenic and Gold-Containing Stibnite Ore Using Slurry Electrolysis

Yonglu Zhang,Chengyan Wang,Baozhong Ma,Xiaowu Jie,Peng Xing
DOI: https://doi.org/10.1016/j.hydromet.2019.04.026
IF: 4.217
2019-01-01
Hydrometallurgy
Abstract:This study investigated the leaching and electrowinning of antimony from a complex, high arsenic and gold containing stibnite concentrate ore (As-Au-Sb ore) using slurry electrolysis (SE). The results indicated that the leaching efficiency of antimony was higher than 98%, and those of iron and arsenic were about 5.50% and 1.14%, respectively. An energy consumption (Ah) of 1.1 times the 'benchmark' value, a duration of 6 h, temperature of 60 degrees C, 30 g/L HCl, 5 g/L Fe, 30 g/L antimony, and an anodic current density of 80 A/m(2) were found to be the optimal experimental conditions. The SE selectively leached antimony, while gold and arsenic were retained in the residue as a raw material for further gold extraction. The antimony content in the cathode antimony was > 98%, and arsenic content was less than or equal to 0.21%. The As-Au-Sb ore consisted of stibnite (Sb2S3), pyrite (FeS2), arsenopyrite (FeAsS), and quartz (SiO2), along with a small amount of muscovite (KAl2(AlSi3O10)(OH)(2)) and other gangue phases. Antimony mainly occurred in stibnite. During the SE, stibnite disappeared, leaving behind elemental sulfur. We proposed a comprehensive procedure for the separation and recovery of antimony from the As-Au-Sb ore. In this process, antimony was recovered in a single step in the form of cathode antimony (> 98%), thereby resolving the technical problem of antimony and arsenic separation and hence, preventing the contamination of plenty of arsenic soda slag and low-concentration SO2 that exists in the traditional pyrometallurgical process. The process was environmentally friendly and had advantages such as short flow and high resource utilization rate.
What problem does this paper attempt to address?