Study on reduction of dolomitic collophane in southwest China by blast furnace process

JI Jun,XU Yao,GUI Kun,TIAN Qi-feng,WU Yuan-xin,LIANG Yong-zhong,CHI Ru-an
DOI: https://doi.org/10.16283/j.cnki.hgkwyjg.2013.09.005
2013-01-01
Abstract:The reaction process of dolomitic collophane in southwest China by phosphoric acid process with blast furnace was studied to observe effect of the reduction temperature,reduction reaction time,silica-calcium ratio and other process conditions on the reduction efficacy.The results showed that the appropriate operational conditions are the reduction temperature being 1400~1450℃,the reduction time 45~60min.and the silica-calcium ratio 2~3.