Influence of shape and bonding area of specimen on microtensile bond strength of dentin adhesive system

TIAN Fucong,WANG Xiaoyan,YU Ling,GAO Xuejun
DOI: https://doi.org/10.3969/j.issn.1001-3733.2008.02.007
2008-01-01
Abstract:Objective:To investigate effects of shape and bonding area of specimen on microtensile bond strength of dentin adhesive system.Methods:Superficial dentins of twelve human third molars were prepared,and bonded with dentin adhesive and composite resin as indicated by the manufacturers.The specimens were randomly divided into four groups and cut into micro-specimens with different shapes(beam or hourglass) and bonding area(1 mm×1 mm or 2 mm×1 mm)(n=15).The microtensile bond strength was determined with Microtensile Tester and the fractured bonding surfaces were observed under a stereomicroscope.The mean bond strengths were compared using two-way ANOVA test.Results:Microtensile bond strength for beam-shape 1 mm×1 mm group was(31.83±8.62)MPa,for beam-shape 2 mm×1 mm group(28.41±4.54) MPa,for hourglass-shape 1 mm×1 mm group(30.94±6.12) MPa,for hourglass-shape 2 mm×1 mm group(30.91±4.52) MPa.There was no significant difference in microtensile bond strength among the four groups(P>0.05).Three specimens with cohesive failure in dentin were observed in hourglass-shape groups.Conclusion:The microtensile bond strength is not influenced by shape(beam or hourglass shape) and bonding area(1 mm×1 mm or 2 mm×1 mm) of specimen.
What problem does this paper attempt to address?