Reduction of Intermetallic Compounds in Ultrasonic-Assisted Semi-Solid Brazing of Al/Mg Alloys

Zhiwu Xu,Zhengwei Li,Lei Xu,Jiuchun Yan
DOI: https://doi.org/10.1080/13621718.2018.1498657
2019-01-01
Abstract:An ultrasonic-assisted semi-solid brazing method was used to control Mg/Al intermetallic compounds (IMCs). Zn–20.95Al, which has a large semi-solid temperature range of 60°C, was chosen as filler metal. Oxide films on the Al/Mg surfaces were removed despite the semi-solid state of the filler metal at 430°C. Al–Mg–Zn IMCs were observed inside the joint at 667 W and 5 s. The IMCs was reduced as ultrasonication time was prolonged. At high power of 1000 W, short ultrasonication time was needed to guarantee that no IMCs remained inside the joint. Otherwise, new IMCs formed because of serious cavitation erosion on substrates. Ultrasonication time of 20 s was unable to completely eliminate IMCs and solid phases at 423°C.