Microstructure of Ti3AI Intermetallic Matrix Composites Produced by In-Situ Reaction

WEI Zun-jie,WANG Hong-wei,ZHANG Er-lin,ZHANG Hu,ZENG Song-yan
DOI: https://doi.org/10.3969/j.issn.1005-0299.2001.01.024
IF: 1.8
2001-01-01
Materials Science and Technology
Abstract:Ti3Al intermetallic matrix composites were prepared using a XD (exothermol deposition) method.The experimental results of composites obtained by XRD, OM, SEM techniques, and electron probe microa-nalysis indicate that in Ti-17Al-0.5C composite the matrix and the reinforcement are Ti3Al and Ti3AlCphases respectively, and the reinforcement has an orientation relationship with the matrix. However, in Ti -17Al-1.5 (2.0) C composites the matrix is Ti3A1, and the reinforcement is TiC coated with a Ti3AlC layer.With increasing C content, morphology of reinforcement changes from undeveloped dendrite to equiaxial den-drite. The microhardness and the elastic modulus of reinforcement and matrix were tested by MPM. The meas-ured results show that the microhardness and the elastic modulus of TiC and Ti3AlC are higher than that of thematrix Ti3Al. The microhardness and the elastic modulus of reinforcement and matrix have little variation withincreasing C content.
What problem does this paper attempt to address?