Abstract:The carboxymethyl cellulose(CMC) is prepared by wastepaper as raw material.The effect of composition of dispersant,alkalization temperature,time,the usage of base and chloroacetic acid,etherification temperature,etc. on viscosity of product are discussed.The results showed that when the 85% ethanol was used as dispersant,the wastepaper was alkalified at 35 ℃ for 90 min,and etherified at 75 ℃ for 150 min and the mass ratio of wastepaper to sodium hydroxide to chloroacetic acid was 1.0∶(0.9)∶1.2,the best quality of CMC product was obtained.Therein,the degree of substitution was 0.6,the mass fraction of available composition was 85%,the moisture was 10% and chloride was 4%,the viscosity of 2% CMC solution was above 500 mPa·s.