Thermal-Induced Dielectric Switching with 40K Wide Hysteresis Loop Near Room Temperature.

Yang-Hui Luo,Chen,Dan-Li Hong,Xiao-Tong He,Jing-Wen Wang,Bai-Wang Sun
DOI: https://doi.org/10.1021/acs.jpclett.8b00597
IF: 6.888
2018-01-01
The Journal of Physical Chemistry Letters
Abstract:A thermal-induced dielectric switching has been realized in two ion-pair crystal [C2H6N5]+·[H2PO4]- (1, C2H6N5 = 3,5-diamino-1,2,4-triazolinium) through single-crystal-to-single-crystal phase transition (SCSC-PT). Upon cooling from room temperature, the 1D cation stripes that are composed of [C2H5N5]+ cations have undergone a 90° sharp rotation around the c axis, accompanied by the transition of crystal stacking from loose unparallel (dynamic state) to compression parallel (static state) and reorientation of dipoles on the [C2H5N5]+ cation, which thus resulted in high dielectric state to low dielectric state transformation. While on the warming run, the reverse process was rather sluggish, resulting in a reversible dielectric switching with ultralarge (about 40K wide) hysteresis loop near room temperature. It is thought that the large-sized polar cation stripes have a predominant influence on the switching properties of 1.
What problem does this paper attempt to address?