Enhanced Emission of Encaged-Oh--Free Ca12(1-X)Sr12xal14o33:0.1% Gd3+ Conductive Phosphors Via Tuning the Encaged-Electron Concentration for Low-Voltage Feds

Meng Zhang,Yuxue Liu,Jian Yang,Hancheng Zhu,Duanting Yan,Xinyang Zhang,Chunguang Liu,Changshan Xu,Hong Zhang
DOI: https://doi.org/10.1039/c7cp01064h
IF: 3.3
2017-01-01
Physical Chemistry Chemical Physics
Abstract:Encaged-OH--free Ca12(1-x)Sr12xAl14O33:0.1%Gd3+ conductive phosphors were prepared through a melt-solidification process in combination with a subsequent heat treatment. Absorption spectra showed that the maximum encaged-electron concentration was increased to 1.08 × 1021 cm-3 through optimizing the doping amount of Sr2+ (x = 0.005). Meanwhile, FTIR and Raman spectra indicated that pure Ca11.94Sr0.06Al14O33:0.1%Gd3+ conductive phosphor without encaged OH- and C22- anions was acquired. For the conductive powders heat-treated in air for different times, the encaged-electron concentrations were tuned from 1.02 × 1021 to 8.3 × 1020 cm-3. ESR, photoluminescence, and luminescence kinetics analyses indicated that the emission at 312 nm mainly originated from Gd3+ ions surrounded by encaged O2- anions, while Gd3+ ions surrounded by encaged electrons had a negative contribution to the UV emission due to the existence of an energy transfer process. Under low-voltage electron-beam excitation (3 kV), enhanced cathodoluminescence (CL) of the conductive phosphors could be achieved by tuning the encaged-electron concentrations. In particular, for the encaged-OH--free conductive phosphor, the emission intensity of the CL was about one order of magnitude higher than that of the conductive phosphor containing encaged OH- anions. Our results suggested that the encaged-OH--free conductive phosphors have potential application in low-voltage FEDs.
What problem does this paper attempt to address?