Template in situ inducing dispersion of nickel on SBA-15 for methane reforming with carbon dioxide

Jing Wang,Tengfei Zhang,Zhongxian Song,Ping Ning,Kaixian Long,Bin Zhao,Jianhong Huang,Qiulin Zhang
DOI: https://doi.org/10.1007/s11164-017-3232-9
IF: 3.134
2017-01-01
Research on Chemical Intermediates
Abstract:Highly dispersed Ni/SBA-15 catalysts were prepared via template extraction with varying different extraction times (Ni/S- x , x = 0.5, 3.5, 6.5 h) for methane reforming with carbon dioxide. Based on the various characterization results and initial activity evaluation, Ni/S-3.5 h catalyst showed the best catalytic performance. Compared with the catalyst prepared via template calcination (Ni-S), Ni/S-3.5 h catalyst held steady with CH 4 and CO 2 conversions while those of the Ni-S catalyst respectively decreased by 15 and 11% during the long-term stability test at 700 °C for 50 h. As TEM and TG–DSC results confirmed, Ni particles in spent Ni/S-3.5 h catalyst stayed well-dispersed with size slightly increasing from an initial 3.9–4.1 nm and nearly no carbon deposition was observed. On the contrary, Ni-S catalyst was subjected to sintered metal particles (increased from 11.6 to 18 nm) and formed carbon fibers. The prominent resistance to sintering and coking over stable Ni/S-3.5 h catalyst was attributed to the high dispersion and strengthened metal-support interaction induced via the residual in situ templates.
What problem does this paper attempt to address?