Corrosion resistance of ultra-high purity porous alumina ceramic support

wu qin,binglong lei,cheng peng,jianqing wu
DOI: https://doi.org/10.1016/j.matlet.2014.12.082
IF: 3
2015-01-01
Materials Letters
Abstract:An ultra-high purity porous alumina ceramic support was prepared by boehmite-coated alumina powders at a relatively low temperature. Its corrosion resistance in 20wt% H2SO4 and 10wt% NaOH hot solutions for 2 to 8h was investigated. After corrosion in H2SO4 solution for 8h, the mass loss was only 0.55%, the flexural strength decreased by 9.85% and the open porosity increased from 41.14% to 47.25%. Meanwhile, the average pore diameter increased from 1.22μm to 1.60μm. While in NaOH solution for 8h, the mass of the support and the flexural strength were diminished by 0.48% and 8.08%, the open porosity and the average pore size were increased to 46.48% and 1.49μm. The permeability increases from 7.18×10−10m2 to 1.35×10−9m2 and 1.25×10−9m2, respectively, after acidic and alkaline corrosion for 8h. The support shows an excellent corrosion resistance.
What problem does this paper attempt to address?