Abstract:ABSTRACTCorrosion fatigue and electrochemical tests under proportional loading and non‐proportional loading were conducted on 304 stainless steel in 0.63 mol L−1 NaCl solution at room temperature. Two biaxial loading paths were applied to study the effect of proportional loading and non‐proportional loading on corrosion fatigue behaviour. Surface and fractographic observations of multiaxial corrosion fatigue specimens were carried out by scanning electron microscopy. It was shown that proportional loading had a more significant effect on the occurrence of local corrosion compared with non‐proportional loading because the continuous rotation of the principal stress plane under non‐proportional loading inhibits the pit formation.
What problem does this paper attempt to address?