Abstract:Deactivation and regeneration of supported skeletal Ni catalyst applied to hydrogenation of indene and styrene in fixed-bed reactor were investigated. The significant aggregation of skeletal Ni and formation of coke precursors were the main reasons for deactivation of catalyst. Furthermore, TG-DTA, XRD, SEM, BET and H2-TPR were utilized to characterize the regenerated catalysts and calcining the spent catalysts in air at 550°C for 3h and then reducing in H2 at 450°C for 3h under 240h−1 (GHSV) could recover its activity according to hydrogenation evaluation results.